When you qualify a weld procedure you need to do your homework in advance to determine, "What do I want my preheat/interpass temperature to be on my final document?" Typically, you would take your essential variable for preheat (25°), add that to your desired preheat temperature for the document to get your target preheat for the test (example: 32° is desired + 25° essential variable = 57° target actual preheat).
Now that you know your target, 57°, this is what transpires: Plates/pipes are cut for testing (temp goes up). Plates/pipes are beveled (temp goes up). Plates/pipes are cleaned up with a grinder (temp goes up). Plates/pipes are tacked and ready (temp goes up). Now you've got a weldment ready to weld and the temperature of that weldment is, let's say, 97°. Before you start the root pass, you need to bring that temperature of the weldment down to be closer to your target temp of 57°.
There are a lot of ways to bring that temp down. I've set the weldment outside in the cold Minnesota air over night, I've placed weldments in the "Beer Fridge", I've even placed them in the Freezer (She hates that one the most). You need to bring that weldments temperature down as close as you can to the 57° target. Once you do, the root pass can be struck.
And yes, all my Boss's thought I was insane.